In Fe-Fe3C phase diagram, the eutectoid composition is 0.8 weight % of carbon at 725 °C. The maximum solubility of carbon in αferrite phase is 0.025 weight % of carbon. A steel sample, having no other alloying element except 0.5 weight % of carbon, is slowly cooled from 1000 °C to room temperature. The fraction of pro-eutectoid αferrite in the above steel sample at room temperature is
Solution :
The correct option is 0.387.
To find the fraction of pro-eutectoid -ferrite in a steel sample containing 0.5 wt% C, we apply the lever rule just above the eutectoid temperature (725 °C).
Let the given carbon composition of the steel sample be .
The eutectoid composition is (which represents the carbon concentration in the austenite phase just before it transforms).
The maximum solubility of carbon in the pro-eutectoid -ferrite phase at the eutectoid temperature is .
Since the steel sample has 0.5 wt% C (which is less than the eutectoid composition of 0.8 wt% C), it is a hypoeutectoid steel. Upon slow cooling from the austenite region (1000 °C), pro-eutectoid ferrite () starts to nucleate and grow along the austenite grain boundaries. This growth continues until the temperature reaches just above the eutectoid temperature (725 °C), where the remaining austenite reaches the eutectoid composition (0.8 wt% C).
The weight fraction of pro-eutectoid ferrite () just before the eutectoid reaction is determined using the lever rule in the () two-phase region:
Substituting the given values into the equation:
This fraction of pro-eutectoid ferrite remains stable and unchanged down to room temperature.
Completely free for students. Educators & coaching institutes get 2 months free Pro trial to create tests.
Access unlimited practice questions, detailed step-by-step solutions, and exam study materials — completely free for students.
Create and conduct professional online assessments with AI question generation, tab proctoring, and comprehensive batch management.
The GATE 2026 Mechanical Engineering (ME) examination scheduled for 14 February 2026 is one of the most important national-level competitive exams for engineering graduates aspiring for higher education and prestigious career opportunities in PSU and research organizations. Conducted annually at the national level, the GATE Mechanical Engineering paper evaluates candidates on core subjects such as Engineering Mechanics, Thermodynamics, Fluid Mechanics, Strength of Materials, Manufacturing Processes, and Machine Design, along with General Aptitude and Engineering Mathematics. This examination is a gateway for admission into M.Tech/Ph.D. programs at IITs, NITs, IISc, and other top institutions, as well as recruitment in major Public Sector Undertakings (PSUs) like ONGC, NTPC, BHEL, IOCL, and more. The GATE ME 2026 paper will test conceptual understanding, analytical thinking, and problem-solving ability, making strong preparation essential for success. Candidates are advised to practice previous year papers, mock tests, and focus on conceptual clarity for high scoring performance. This exam on 14/02/2026 is a crucial opportunity for mechanical engineering aspirants to secure their future in academia and industry.
Strengthen your preparation with this GATE 2025 Mechanical Engineering (ME) test, covering core subjects such as thermodynamics, fluid mechanics, strength of materials, theory of machines, and manufacturing engineering. With a well-balanced mix of conceptual and numerical questions, this test helps enhance problem-solving ability and technical understanding. Aligned with the latest exam pattern, it is ideal for improving accuracy, speed, and overall exam readiness.
Copyright © 2026 Combe Labs Private Limited. All Rights Reserved.