Question Details

Match the following sand mold casting defects with their respective causes.




Defect Cause
PBlow hole
1Poor collapsibility
QMisrun
2Mold erosion
RHot tearing
3Poor permeability
SWash
4Insufficient fluidity

Options

A

P-4, Q-3,R-1,S-2

B

P-3,Q-4, R-2, S-1

C

P-2, Q-4,R-1,S-3

D

P-3, Q-4,R-1, S-2

Show Answer
Correct Answer

Solution :

The correct option is P-3, Q-4, R-1, S-2.

To understand why this match is correct, let us analyze each sand mold casting defect and its corresponding cause step-by-step:

1. Blow hole (P) matches with Poor permeability (3)
Blow holes are smooth, round holes or cavities formed on the surface or inside the casting. During pouring, moisture in the sand mold vaporizes to form gases. If the sand mold has poor permeability, these gases cannot escape through the sand pores and instead get trapped inside the molten metal as it solidifies, causing blow holes.

2. Misrun (Q) matches with Insufficient fluidity (4)
A misrun occurs when the liquid metal fails to completely fill the mold cavity, leaving an incomplete casting. This defect is caused by insufficient fluidity of the molten metal, which prevents it from flowing into all the thin sections or corners of the mold before it solidifies.

3. Hot tearing (R) matches with Poor collapsibility (1)
Hot tears (or hot cracks) are tears that occur in the casting as it cools and shrinks during solidification. If the mold has poor collapsibility (meaning it does not easily compress or collapse under the contraction forces of the cooling metal), it restricts the natural shrinkage of the casting, inducing tensile stresses that lead to hot tearing.

4. Wash (S) matches with Mold erosion (2)
A wash is a surface defect characterized by an excess projection of metal on the casting surface. It is caused by mold erosion, where the high-velocity flow of incoming molten metal washes away or erodes the loose sand from the mold surface (specifically near the gate or runner), creating cavities that then fill with metal.

Transparent Access on Mindyard

Built for Learners & Educators Alike

Completely free for students. Educators & coaching institutes get 2 months free Pro trial to create tests.

FREE FOR STUDENTS

Practice & Learn Free for Students

Access unlimited practice questions, detailed step-by-step solutions, and exam study materials — completely free for students.

  • Unlimited mock tests & question bank practice
  • Full access to curated study library & formula notes
  • 100% free for students • No credit card required
2 MONTHS FREE TRIAL

Educators & Coaching Institutes

Create and conduct professional online assessments with AI question generation, tab proctoring, and comprehensive batch management.

  • AI question uploader & rapid test generator
  • Anti-cheating tab proctoring & performance reports
  • Full Pro access free for 60 days • No upfront commitment
Discover more resources

You may also like

Mock Tests

View All
  • GATE
  • intermediate
  • 3 hours
  • mechanical engineering

The GATE 2026 Mechanical Engineering (ME) examination scheduled for 14 February 2026 is one of the most important national-level competitive exams for engineering graduates aspiring for higher education and prestigious career opportunities in PSU and research organizations. Conducted annually at the national level, the GATE Mechanical Engineering paper evaluates candidates on core subjects such as Engineering Mechanics, Thermodynamics, Fluid Mechanics, Strength of Materials, Manufacturing Processes, and Machine Design, along with General Aptitude and Engineering Mathematics. This examination is a gateway for admission into M.Tech/Ph.D. programs at IITs, NITs, IISc, and other top institutions, as well as recruitment in major Public Sector Undertakings (PSUs) like ONGC, NTPC, BHEL, IOCL, and more. The GATE ME 2026 paper will test conceptual understanding, analytical thinking, and problem-solving ability, making strong preparation essential for success. Candidates are advised to practice previous year papers, mock tests, and focus on conceptual clarity for high scoring performance. This exam on 14/02/2026 is a crucial opportunity for mechanical engineering aspirants to secure their future in academia and industry.

  • GATE
  • intermediate
  • 3 hours
  • mechanical engineering

Strengthen your preparation with this GATE 2025 Mechanical Engineering (ME) test, covering core subjects such as thermodynamics, fluid mechanics, strength of materials, theory of machines, and manufacturing engineering. With a well-balanced mix of conceptual and numerical questions, this test helps enhance problem-solving ability and technical understanding. Aligned with the latest exam pattern, it is ideal for improving accuracy, speed, and overall exam readiness.

Ask AI Tutor
5 left
Q1 View Question & Options
AI Tutor is solving this question...
Reading question context & options...
Ask your own doubt or choose a quick prompt: